solid forge — Filament drying temperatures and times | solid-forge.com
Read per-material drying temperatures and times in one table and note the warning not to exceed them.
The quick answer: PLA, rPLA and Woodfill dry at 45 °C for 6 hours; PVB at 45 °C for 8 hours; PETG in all versions at 55 °C for 6 hours; TPU at 60 °C for 4–6 hours; PP Carbon Fiber and Glass Fiber at 70 °C for 2–4 hours; ASA at 80 °C for 4 hours; PC Blend at 85 °C for 5 hours; PC Blend Carbon Fiber at 90 °C for 4 hours; PC Space Grade at 90 °C for 4–6 hours; PA11 Carbon Fiber at 90 °C for 6 hours; and PEI at 150 °C for 8 hours.
The list contains eleven material entries spread over seven temperature levels: 45, 55, 60, 70, 80, 85, 90 and 150 °C. The lowest level is shared by four materials and the highest by one, which is why the range is so wide.
Reading the table correctly means treating each row as a pair. A temperature without its time, or a time without its temperature, is not the recommendation. The reference is explicit that the temperature must not be exceeded, and equally explicit that the time should not be exceeded to avoid overdrying.
The consequence of exceeding the temperature is described in mechanical terms: the filament softens and sticks together. That is a failure of the filament itself, not only of the print, and it happens inside the drying appliance before any printing is attempted.
The consequence of exceeding the time is overdrying. The schedules therefore function as windows. Where a range is given — 4–6 hours for TPU and PC Space Grade, 2–4 hours for PP Carbon Fiber and Glass Fiber — the range is the permitted window, not an invitation to pick the longest value by default.
Several materials share a temperature but not a time. PLA, rPLA and Woodfill are at 45 °C for 6 hours while PVB is at 45 °C for 8 hours, so the temperature alone does not determine the schedule. PC Blend Carbon Fiber is at 90 °C for 4 hours while PA11 Carbon Fiber is at 90 °C for 6 hours, the same pattern at the top of the middle range.
On narrow screens, swipe or scroll the plate sideways.
The PC family splits by variant rather than sharing one row. PC Blend is 85 °C for 5 hours, PC Blend Carbon Fiber is 90 °C for 4 hours, and PC Space Grade is 90 °C for 4–6 hours. Anyone drying a PC filament needs to identify the exact version first.
PETG is the opposite case: all versions share a single schedule of 55 °C for 6 hours. The reference does not distinguish between PETG variants, so the same pair applies across the family.
PEI stands alone at 150 °C for 8 hours. It is the highest temperature and the longest time in the reference, and it is far above every other entry. Nothing else in the list comes within 60 °C of it.
The table does not include spool limits, and that omission is deliberate here: the spool question is handled separately because it can override the filament schedule. The old black Prusament spool caps at 45 °C and the old grey one at 90 °C because of its hub glue.
In practice, the lookup order is: find the material row, note both numbers, then check the spool. If the spool ceiling is lower than the filament temperature, the spool governs until the documented workaround is applied.
The arithmetic over the table is simple and worth stating: eleven entries, seven temperature levels, a 105 °C span from 45 to 150 °C, and a 6-hour span in time from 2 to 8 hours. Those figures describe the list, not the performance of any dryer.
Further reading