solid forge — Filament drying temperatures and times | solid-forge.com

Drying temperatures and times

solid forge — Filament drying temperatures and times | solid-forge.com

This reference lists the recommended drying temperature and time for common FFF filaments, from PLA at 45 °C to PEI at 150 °C. It also covers what to check on the spool before heating and how to store filament afterwards. Use the table to look up your material, then read the spool notes before you start.

What temperatureand how many hoursWhat happens if Igo above theDoes the spool needpreparation beforeWhich drying methodshould I use?How should filamentbe stored afterWhat should Iverify before
A map of this guide's sections

01

The schedule is a pair

Every entry in the reference is a temperature and a time together. Reading only the temperature or only the hours loses half of the constraint.

02

The spool has its own limit

Old black Prusament spools are safe to 45 °C unless an M4x65 screw holds the sides together; old grey spools are glued to 90 °C. The lower of filament and spool limits governs.

03

The appliance must be verified

Home ovens drift and need an external thermometer; food dehydrators often cap low and must be checked before purchase against the schedule you need.

What temperature and how many hours should I dry a given FFF filament?

Look up your material in the table below; the schedule is a fixed pair of temperature and time, and both bounds matter.

The recommendations group into a low band (45 °C for PLA, rPLA, Woodfill and PVB), a middle band (55 °C for PETG, 60 °C for TPU, 70 °C for PP Carbon Fiber and Glass Fiber), a high band (80 °C for ASA, 85 °C for PC Blend), and a very high band (90 °C for PC Blend Carbon Fiber, PC Space Grade and PA11 Carbon Fiber, and 150 °C for PEI).

Times run from 2–4 hours for PP Carbon Fiber/Glass Fiber and 4 hours for TPU, ASA and PC Blend Carbon Fiber, through 4–6 hours for PC Space Grade and TPU's upper bound, to 6 hours for PLA, Woodfill, PETG, PC Blend and PA11 Carbon Fiber, 8 hours for PVB and PEI, and 5 hours for PC Blend.

Both numbers are limits. The temperature ceiling protects the spool and the filament from softening and fusing; the time window protects against overdrying. A schedule is not a suggestion to go hotter for less time.

  • PLA, rPLA, Woodfill: 45 °C for 6 hours
  • PVB: 45 °C for 8 hours
  • PETG (all versions): 55 °C for 6 hours
  • TPU: 60 °C for 4–6 hours
  • PP Carbon Fiber / Glass Fiber: 70 °C for 2–4 hours
  • ASA: 80 °C for 4 hours
  • PC Blend: 85 °C for 5 hours

Material bands at a glance

Low band

45 °C materials

PLA, rPLA, Woodfill and PVB all dry at 45 °C. PLA, rPLA and Woodfill take 6 hours; PVB takes 8. This is also the safe ceiling for old black Prusament spools.

Middle band

55–70 °C materials

PETG (all versions) at 55 °C for 6 hours, TPU at 60 °C for 4–6 hours, and PP Carbon Fiber/Glass Fiber at 70 °C for 2–4 hours.

High band

80–85 °C materials

ASA at 80 °C for 4 hours and PC Blend at 85 °C for 5 hours. Old grey Prusament spools remain within their 90 °C glue rating here.

Very high band

90 °C materials

PC Blend Carbon Fiber (4 h), PC Space Grade (4–6 h) and PA11 Carbon Fiber (6 h) all sit at 90 °C. At this level the grey spool glue is at its rated limit.

Top

PEI at 150 °C

The highest schedule in the reference: 150 °C for 8 hours. No standard spool hardware is documented as safe at this level, so the spool question must be resolved first.

Appliance

Matching the tool to the schedule

A dryer or professional oven with a verified setpoint covers the range; a home oven needs an external thermometer; a food dehydrator must be checked for its maximum before purchase.

The schedule is a ceiling and a window at once: too hot fuses the loops, too long overdries the filament.
The spool can fail before the filament does — check the hub before you set the temperature.

Drying schedule by material

MaterialTemperatureTimeSpool note
PLA / rPLA / Woodfill45 °C6 hoursOld black Prusament spool is at its 45 °C ceiling
PVB45 °C8 hoursSame 45 °C ceiling applies
PETG (all versions)55 °C6 hoursAbove the black-spool ceiling; use a screw or another spool
TPU60 °C4–6 hoursAbove the black-spool ceiling
PP Carbon Fiber / Glass Fiber70 °C2–4 hoursAbove the black-spool ceiling
ASA80 °C4 hoursAbove the black-spool ceiling
PC Blend85 °C5 hoursBelow the 90 °C grey-spool glue rating
PC Blend Carbon Fiber / PC Space Grade / PA11 Carbon Fiber90 °C4 / 4–6 / 6 hoursGrey-spool glue at its rated limit
PEI150 °C8 hoursWell above both documented spool ceilings
Visitor task: Look up the recommended drying temperature and time for a specific filament1 itemA concrete procedure in this guide
Eleven material entries, seven temperature levels, and times from 2 to 8 hours — the time span is 6 hours end to end.

Questions before you start drying

Can I dry PETG at 60 °C instead of 55 °C to save time?
No. The reference gives 55 °C for 6 hours for PETG (all versions) and states that exceeding the recommended temperature softens the filament and makes it stick together. Shortening the time does not compensate for the higher temperature, because the two limits protect different failure modes.
My spool is an old black Prusament one and my filament needs 90 °C. What do I do?
The old black spool is safe only up to 45 °C. The documented workaround is a screw with a thread of at least 65 mm, such as an M4x65 tightened with a 3.5 mm Allen key, to hold the two sides together. Without that, the spool limits the job to 45 °C regardless of the filament schedule.
Can I use a food dehydrator for every filament in the table?
Only if its maximum temperature covers the schedule you need. Food dehydrators usually have only low temperatures, so the filament's drying temperature should be checked before purchasing one. A dehydrator that stops below 70 °C cannot serve PP Carbon Fiber, ASA, PC Blend, PA11 Carbon Fiber or PEI.
Is a home oven accurate enough without a separate thermometer?
The reference says home ovens do not have a very precise temperature measurement, so an external thermometer should be used to correct the temperature if necessary. The dial setting alone is not treated as reliable, and the correction is made against the reading rather than the setpoint.

Source basis

One explicit check over the listed facts: the eleven material entries run from 45 °C to 150 °C, a 105 °C span, and from 2 to 8 hours, a 6-hour span.