solid forge — Filament drying temperatures and times | solid-forge.com

solid forge — Filament drying temperatures and times | solid-forge.com

Spool preparation and post-drying storage

Decide whether a spool needs preparation before heating and how to store filament after drying.

The quick answer: some spools need preparation and some do not. Old black Prusament spools are safe only up to 45 °C; above that, a screw with a thread of at least 65 mm — such as an M4x65 tightened with a 3.5 mm Allen key — holds the two sides together. Old grey Prusament spools are glued to the cardboard centre with adhesive rated to 90 °C, so no screw is needed if that temperature is not exceeded.

The two rules answer different failure modes. The black spool fails mechanically when heated past its limit, which is why the workaround is a mechanical fastener. The grey spool's limitation is the adhesive, which is why its ceiling is a temperature rather than a fastener.

Preparation therefore starts with identification. Before setting any drying temperature, determine which spool type the filament is on. The filament schedule may call for 90 °C or 150 °C while the spool tolerates far less.

If the spool is an old black Prusament type and the schedule is above 45 °C, the documented option is the screw. The specification is precise: a thread of at least 65 mm, with M4x65 given as the example and a 3.5 mm Allen key as the tool. Without it, the job is capped at 45 °C.

If the spool is an old grey Prusament type, no screw is needed as long as 90 °C is not exceeded. At exactly 90 °C the glue is at its rated limit, and the reference describes the rating as withstanding up to 90 °C. Schedules above that level are outside the documented range for this spool.

For spools not covered by these two notes, the reference gives no specific hardware limit. The conservative reading is that an undocumented spool has an unknown ceiling, and the filament schedule should not be assumed to apply to the hardware.

Post-drying storage is not specified in the source material in terms of containers or desiccant quantities. What the source does establish is that the drying limits apply whenever drying is performed, so a spool that is dried, stored and later re-dried goes through the same checks each time.

That repetition matters because the spool condition does not reset. A black spool that needed a screw for its first 90 °C cycle needs it again for the second. The glue on a grey spool does not become more heat-resistant with use.

The practical post-drying rule is to keep the filament dry and to repeat the documented schedule if moisture returns, rather than inventing a longer or hotter cycle. The overdrying warning applies to repeat cycles exactly as it applies to the first.

The signature mark of this site, drawn as a plate

On narrow screens, swipe or scroll the plate sideways.

There is also an ordering point. Preparation happens before heating, not during it. Once the spool is in the appliance and the temperature is rising, a missing screw or an overestimated glue rating cannot be corrected without stopping the cycle.

A simple checklist follows from the two documented cases: identify the spool, compare its ceiling with the filament schedule, apply the screw if the spool is an old black Prusament type and the schedule exceeds 45 °C, and confirm the grey spool stays at or below 90 °C.

The arithmetic here is small but decisive: the black spool's 45 °C ceiling is 45 °C below the 90 °C group and 105 °C below PEI's 150 °C. Those gaps are why the spool check has to come before the temperature is set.

Begin by matching the filament to its schedule before touching any appliance. PLA and rPLA, along with Woodfill, are listed at 45 °C for 6 hours, while PVB needs the same 45 °C but for 8 hours. PETG in all versions is rated at 55 °C for 6 hours. Write the number down and compare it with the spool ceiling, since the hardware check comes first and a mismatch means the cycle cannot run as listed.

Flexible and filled materials sit a little higher. TPU is given 60 °C for 4 to 6 hours, and PP Carbon Fiber or Glass Fiber at 70 °C for 2 to 4 hours. These are short cycles, so timing matters as much as temperature. Set the appliance, confirm the reading with an external thermometer, and stop at the upper end of the listed range rather than extending it to chase a result the reference does not promise.

Engineering blends climb further. ASA is listed at 80 °C for 4 hours and PC Blend at 85 °C for 5 hours. PC Blend Carbon Fiber and PC Space Grade both reach 90 °C, for 4 hours and 4 to 6 hours respectively. Before selecting any of these, re-check the spool: an old black Prusament spool is safe only to 45 °C, so the documented screw, a thread of at least 65 mm such as an M4x65, becomes mandatory.

The top of the range needs the most caution. PA11 Carbon Fiber is rated at 90 °C for 6 hours and PEI at 150 °C for 8 hours. PEI's figure is far above every spool ceiling discussed here, which makes the hardware check decisive rather than routine. Old grey Prusament spools rely on adhesive rated to 90 °C, so no screw is needed below that temperature, but 150 °C is well outside the documented range for that hardware.

Two limits frame every cycle. Do not exceed the recommended temperature, because the filament softens and sticks together, and do not exceed the recommended time, because overdrying damages the material. A home oven's temperature measurement is imprecise, so place an external thermometer inside and correct the setting if the reading drifts. A food dehydrator often tops out at low temperatures, so verify its range covers the filament's figure before buying one.

After drying, keep the filament dry and repeat the same documented schedule if moisture returns, rather than inventing a hotter or longer cycle. Each re-drying run goes through the same checks: identify the spool, compare its ceiling with the filament schedule, fit the screw if needed, and confirm the thermometer reading before trusting the appliance's dial. A worked example: PETG at 55 °C on an old black spool needs no screw, but PC Blend at 85 °C on the same spool does.

  • Identify the spool type before heating
  • Old black Prusament: 45 °C ceiling; fit an M4x65 screw above it
  • Old grey Prusament: 90 °C glue rating, no screw needed below it
  • Re-check the spool on every drying cycle, not only the first

Questions and answers

What exactly do I need to hold an old black Prusament spool together?
A screw with a thread of at least 65 mm. The reference gives an M4x65 screw tightened with a 3.5 mm Allen key as the example. The purpose is to hold the two sides of the spool together so the hardware survives temperatures above its 45 °C safe limit.
Does the grey spool glue mean I can go above 90 °C safely?
No. The adhesive is described as withstanding up to 90 °C, so 90 °C is the top of its rated range rather than a margin below a higher limit. The reference's wording is that no screw is needed if this temperature is not exceeded, which places the ceiling at 90 °C.
Do I need to repeat the spool check after the filament has been stored?
Yes, on every drying cycle. The spool hardware does not change with storage: a black spool still needs the screw above 45 °C and a grey spool is still limited by its 90 °C glue. The drying schedule is repeated when moisture returns, and the preparation step repeats with it.